Related Books
Language: en
Pages: 568
Pages: 568
Type: BOOK - Published: 1990 - Publisher: ASM International(OH)
A reference for materials scientists that can be used to find the effects of various corrosive media and processing variables on the stress-corrosion cracking a
Language: en
Pages: 821
Pages: 821
Type: BOOK - Published: 2002-01-01 - Publisher: ASM International
Contains more than 1400 curves, almost three times as many as in the 1987 edition. The curves are normalized in appearance to aid making comparisons among mater
Language: en
Pages: 544
Pages: 544
Type: BOOK - Published: 1985-12-31 - Publisher: ASM International
Contains more than 500 fatigue curves for industrial ferrous and nonferrous alloys. Also includes an explanation of fatigue testing and interpretation of test r
Language: en
Pages: 803
Pages: 803
Type: BOOK - Published: 2018-09-28 - Publisher: Elsevier
Corrosion Atlas: A Collection of Illustrated Case Studies, Third Edition includes 679 case histories divided over 135 materials in 13 material groups, 25 system
Language: en
Pages: 212
Pages: 212
Type: BOOK - Published: 2021-11-28 - Publisher: Elsevier
Corrosion engineers today spend enormous amounts of time and money searching multiple detailed sources and variable industry-specific standards to locate known